Material Notes:
Surlyn® 8120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neutralization levels for this grade are optimized to deliver higher hardness and stiffness compared with other sodium ionomer grades. In golf ball covers, the resin is used primarily in blends with other grades to improve cut resistance and impact durability, as well as increased resilience and coefficient of restitution. The resin also offers high clarity and good abrasion resistance. It can be injection or blow molded, and is processable by extrusion into sheets or shapes.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
ASTM D2240
Tensile Strength, Ultimate 28.8 MPa
4180 psi
ASTM D638
Tensile Strength, Yield 4.50 MPa
653 psi
50 mm/min cross speed; ASTM D638
Elongation at Break 660 %
660 %
ASTM D638
Flexural Modulus 0.0490 GPa
7.11 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Tensile Impact Strength 490 kJ/m²
233 ft-lb/in²
ASTM D1822S
Thermal Properties Metric English Comments
Melting Point 78.0 °C
172 °F
DSC
Vicat Softening Point 51.0 °C
124 °F
Rate B, ASTM D1525-70