Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 693 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 693 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 693 is a super clear polyester film pretreated on one side to promote adhesion with improved handleability.General Product Info: Melinex® 693 is a high clarity, non-yellow base with excellent adhesion on the pretreated surface.Typical Applications: Melinex® 693 is a very unique film with ultra high clarity for a wide range of display applications.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 245 MPa
35600 psi
ASTM D882A
Film Tensile Strength at Break, TD 274 MPa
39800 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 0.50 %

@Thickness 0.0361 mm
0.50 %

@Thickness 0.00142 in
ASTM D1003