Film Tensile Strength at Break, MD 245 MPa
35600 psi
ASTM D882A
DuPont Teijin Films Melinex® 693 Polyester Film
Melinex® 693 is a super clear polyester film pretreated on one side to promote adhesion with improved handleability.General Product Info: Melinex® 693 is a high clarity, non-yellow base with excel..
Film Tensile Strength at Break, MD 245 MPa
35600 psi
ASTM D882A
DuPont Teijin Films Melinex® 694 Polyester Film
Melinex® 694 is a super clear polyester film pretreated on two sides to promote adhesion with improved handleability.General Product Info: Melinex® 694 is a high clarity, non-yellow base with exce..