DuPont Teijin Films Mylar® 800 Polyester Packaging Film, 48 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® 800 Polyester Packaging Film, 48 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.Melinex® 800 is a clear, non-pretreated base film with high gloss, low haze and excellent processability. Melinex® 800 is available in 48 gauge. Melinex® 800 polyester film is stiffer than polypropylene and also maintains an excellent film thickness profile and roll formation to ensure consistent processability in operations. Melinex® 800 film features good clarity and handling characteristics in metallizing operations. When aluminum metallized, the film exhibits excellent aesthetic quality as well as the best barrier to oxygen and moisture in a flexible film.Melinex® 800 is a polyester film that is compliant with the U.S. Food and Drug Administration regulations under 21 CFR 177.1630, Sections (f), (g),and (h). These sections cover the use of PET in contact with all types of foods (excluding alcoholic beverages) at temperatures up to and above 250°F (including oven baking or cooking) and alcoholic beverages (not to exceed 50 percent by alcohol by volume) at ambient temperatures.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Moisture Vapor Transmission 0.0120 cc-mm/m²-24hr-atm
0.0305 cc-mil/100 in²-24hr-atm
metallized barrier; 2.8 g/100in²-24hr-atm unmetallized barrier; Tested per ASTM F372 at 100°F, 90% RH.
Oxygen Transmission 0.0200 cc-mm/m²-24hr-atm
0.0508 cc-mil/100 in²-24hr-atm
metallized barrier; 6 cc/100in²-24hr-atm unmetallized barrier; Tested per ASTM D1434 at 77°F, 75% RH.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 70 %
70 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
ASTM D1894
Coefficient of Friction, Static 0.50
0.50
ASTM D1894
Film Tensile Strength at Break, MD 222 MPa
32200 psi
ASTM D882A
Film Tensile Strength at Break, TD 269 MPa
39000 psi
ASTM D882A
Optical Properties Metric English Comments
Haze 3.6 %
3.6 %
Gardner; ASTM D1003
Transmission, Visible 88.5 %
88.5 %
ASTM D1003