Material Notes:
Mylar® AHS1 is a strong, tough, and durable PET film with an unusual balance of properties. It is used for many industrial and electrical applications. General Product Info: Mylar® ASH1 has a tensile strength that averages 28,000 psi, has excellent resistance to moisture and most chemicals, and exceptional durability in high-temperature environments. Because it contains no plasticizers Mylar® AHS1 does not become brittle with age under normal conditions.Typical Applications: Mylar® AHS1 is a unique product whose shrinkage and high resistance to deformation make it well suited for applications such as carbon ribbons and electrical insulation.Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 100 %
100 %
ASTM D882A
Film Tensile Strength at Break, MD 193 MPa
28000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 17.5 %
17.5 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Strength 192.6 kV/mm
4891 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 4500 V
4500 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149