DuPont Teijin Films Mylar® M577 Polyester Film, 48 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® M577 Polyester Film, 48 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® Type M577 is a tough, transparent film. A rough surface provides ease of handling, good adhesion, and processability.General Product Info: Mylar® Type M577 film has balanced tensile properties and excellent resistance to moisture and most chemicals. It can withstand temperature extremes from -94 to 302° F. Because it contains no plasticizers, it does not become brittle with age under normal conditionsTypical Applications: Mylar® Type M577 film is used almost exclusively in specialty (DC) capacitors.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 70 %
70 %
ASTM D882A
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 150 °C
302 °F
Maximum Service Temperature, Inert -70.0 °C
-94.0 °F
Shrinkage, MD 2.0 %

@Temperature 150 °C,
Time 1800 sec
2.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 150 °C,
Time 1800 sec
1.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 4.0 %
4.0 %
Transmission, Visible 90 %
90 %
transparent; thickness not quantified