DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mylar® OL22 is a one side heat sealable, polyester film. It can be heat sealed to itself and heat seals well to thermoformed APET/CPET trays and APET coated board. It also heat seals to various other substrates including PVdC, PVC, paper and aluminum foil, but will not seal to polyolefins. The plain or non-heat seal surface of Mylar® OL22 exhibits the properties of standard polyester film. General Product Info: Mylar® OL22 has an exceptionally wide heat seal range, from 220°F to 400°F, with outstanding hot tack properties. The plain surface of Mylar® OL22 can be printed or metallized in the same way as plain polyester film, although the sealable surface makes handling of the film during conversion more critical. The heat seal surface of the film is normally wound on the inside of the roll.Typical Applications: Mylar® OL22 is an excellent film for applications where chemical resistance of the sealant surface is required. It offers excellent thermal properties in freezer to oven applications for lidding applications.Approvals: FDA Food Contact Status - All gauges of Mylar® OL22 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Mylar® OL22 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Water Vapor Transmission 17.1 g/m²/day

@Temperature 38.0 °C
1.10 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 100 %
100 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Coefficient of Friction, Dynamic 0.50
0.50
ASTM D1894
Film Tensile Strength at Break, MD 186 MPa
27000 psi
ASTM D882A
Film Tensile Strength at Break, TD 200 MPa
29000 psi
ASTM D882A
Heat Seal Strength 500 g/25 mm

@Time 1.00 sec
1.10 lb/in

@Time 0.000278 hour
285°C (HS/HS)
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 3.5 %

@Temperature 190 °C,
Time 300 sec
3.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 6.0 %
6.0 %
ASTM D1003
Descriptive Properties Value Comments
Gas Permeability (Base film) 3.1 cc/100 in2
O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal) 16500 in2/lb