Polymer Property : Water Vapor Transmission = 17.1 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 17.1 g/m²/day

@Temperature 38.0 °C
1.10 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
DuPont Teijin Films Mylar® OL22 Polyester Film, 100 Gauge
Product Description: Mylar® OL22 is a one side heat sealable, polyester film. It can be heat sealed to itself and heat seals well to thermoformed APET/CPET trays and APET coated board. It also heat..