DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhesion Pretreated (both sides); available in 750 & 1000 gaugeU2L98W: Low Shrinkage, Adhesion Pretreated (both sides); available in 500 gaugeTypical Applications: Prepaid cards (Magnetic Cards)LabelImagingInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 80 %
80 %
ASTM D882A
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
Film Tensile Strength at Break, TD 205.9 MPa
29870 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.1 %

@Temperature 150 °C,
Time 1800 sec
1.1 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.30 %

@Temperature 150 °C,
Time 1800 sec
0.30 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Gloss 47 %
47 %
60°; ASTM D1003
Descriptive Properties Value Comments
Color 0.1
a
-2.3
b
92
L
Users viewing this material also viewed the following: