Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, MD = 25520 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 740 Gauge
Teijin® Tetoron® HSL is a low shrinkage polyester film with well balanced physical, chemical and optical properties. In addition to the standard, non-pretreated, Teijin® Tetoron® HSL film, the f..
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 150 Gauge
Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe..
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 200 Gauge
Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe..
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 300 Gauge
Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe..
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 400 Gauge
Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe..
Film Tensile Strength at Break, MD 176.0 MPa
25520 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 300 Gauge
Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod..
Copyright © lookpolymers.com All Rights Reserved