Material Notes:
Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminates the need for heat tracing in outdoor applications.Information provided by Duratherm.
Physical Properties Metric English Comments
Density 0.6129 g/cc

@Temperature 316 °C
0.02214 lb/in³

@Temperature 600 °F
0.636 g/cc

@Temperature 288 °C
0.0230 lb/in³

@Temperature 550 °F
0.646 g/cc

@Temperature 260 °C
0.0233 lb/in³

@Temperature 500 °F
0.684 g/cc

@Temperature 204 °C
0.0247 lb/in³

@Temperature 400 °F
0.815 g/cc

@Temperature 37.8 °C
0.0295 lb/in³

@Temperature 100 °F
Kinematic Viscosity 0.40 cSt

@Temperature 260 °C
0.40 cSt

@Temperature 500 °F
0.56 cSt

@Temperature 260 °C
0.56 cSt

@Temperature 500 °F
0.63 cSt

@Temperature 260 °C
0.63 cSt

@Temperature 500 °F
Kinematic Viscosity at 40°C (104°F) 7.7 cSt
7.7 cSt
Kinematic Viscosity at 100°C (212°F) 2.3 cSt
2.3 cSt
Molecular Weight 395 g/mol
395 g/mol
Average
Vapor Pressure 0.0703 bar

@Temperature 204 °C
52.7 torr

@Temperature 400 °F
0.2896 bar

@Temperature 260 °C
217.2 torr

@Temperature 500 °F
0.52676 bar

@Temperature 288 °C
395.10 torr

@Temperature 550 °F
0.5551 bar

@Temperature 316 °C
416.3 torr

@Temperature 600 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 2.18 J/g-°C

@Temperature 37.8 °C
0.520 BTU/lb-°F

@Temperature 100 °F
2.72 J/g-°C

@Temperature 204 °C
0.651 BTU/lb-°F

@Temperature 400 °F
2.93 J/g-°C

@Temperature 260 °C
0.700 BTU/lb-°F

@Temperature 500 °F
3.02 J/g-°C

@Temperature 288 °C
0.721 BTU/lb-°F

@Temperature 550 °F
3.10 J/g-°C

@Temperature 316 °C
0.740 BTU/lb-°F

@Temperature 600 °F
Thermal Conductivity 0.118 W/m-K

@Temperature 288 °C
0.816 BTU-in/hr-ft²-°F

@Temperature 550 °F
0.118 W/m-K

@Temperature 316 °C
0.816 BTU-in/hr-ft²-°F

@Temperature 600 °F
0.121 W/m-K

@Temperature 260 °C
0.840 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.125 W/m-K

@Temperature 204 °C
0.864 BTU-in/hr-ft²-°F

@Temperature 400 °F
1.40 W/m-K

@Temperature 37.8 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 100 °F
Pour Point -57.8 °C
-72.0 °F
Flammability Test 370
370
Fire Point, °F
675
675
Autoignition Temp, °F
Flash Point 165 °C
329 °F
Descriptive Properties Value Comments
Distillation range at 10% 613
Distillation Range at 90% 784
Max Bulk Temp (°F) 600
Max Film Temp (°F) 650