Polymer Property : Thermal Conductivity = 1.40 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.40 - 1.60 W/m-K

@Temperature 600 °C
9.72 - 11.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS PBK D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This moldable contains a phosphate binding agent and has a low silica cont..
Thermal Conductivity 1.40 - 1.60 W/m-K

@Temperature 600 °C
9.72 - 11.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material
Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo..
Thermal Conductivity 1.40 - 1.60 W/m-K

@Temperature 1200 °C
9.72 - 11.1 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable
Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values ..
Thermal Conductivity 1.40 - 1.60 W/m-K

@Temperature 600 °C
9.72 - 11.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS PBK Moldable Refractory Material
Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at..
Thermal Conductivity 1.40 W/m-K

@Temperature 37.8 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 100 °F
Duratherm LT Paraffinic Heat Transfer Fluid
Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat..
Thermal Conductivity 1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628..
Thermal Conductivity 1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76..