Dymax 955 Potting and Encapsulation Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 955 Potting and Encapsulation Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 955 Potting and Encapsulation AdhesiveHigh strength with superior adhesion to steel, aluminum and glass. Cure Type: UV or Heat
Physical Properties Metric English Comments
Viscosity 4000 cP
4000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.8 MPa
2000 psi
Processing Properties Metric English Comments
Cure Time <= 0.0833 min
<= 0.00139 hour
Descriptive Properties Value Comments
Cure Depth 0.5 in.