Dymax Sure Cure™ 984 Conformal Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name Sure Cure™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax Sure Cure™ 984 Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 984 Sure Cure™ Conformal CoatingTough, glossy fluorescing 2-part system, shadow cures at room temperature. Cure Speed (fpm): 2 - 5 (72 hr shadow) Cure Type: UV, Chemical, Air
Physical Properties Metric English Comments
Viscosity 100 cP
100 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.7 MPa
6200 psi
Descriptive Properties Value Comments
Cure Depth 0.015 in.