Dynasol Solprene® 411 Thermoplastic Rubber SBS Dry

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Dynasol
Trade Name Solprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 411 Thermoplastic Rubber SBS Dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene 411 is a 70/30 butadiene/styrene thermoplastic copolymer, polymerized in solution and has a radial structure.This product is available in:S 411 porous crumbS 411M powder form dusted with amorphous silicaApplications:Bitumen modificationFootwearMechanical rubber goodsPlastic modificationadhesivesInformation provided by Dynasol
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D-5668
Viscosity 2200 cP

@Temperature 180 °C
2200 cP

@Temperature 356 °F
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer)
Viscosity Measure 28 cSt
28 cSt
Toluene solution viscosity 5,23%; NM 300-11
Mechanical Properties Metric English Comments
Penetration <= 50
<= 50
at 25°C dmm, Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer); ASTM D-5-86
Thermal Properties Metric English Comments
Ring & Ball Softening Point >= 130 °C
>= 266 °F
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer); ASTM D-36
Chemical Properties Metric English Comments
Styrene Content 30 %
30 %
on polymer; ASTM D-5775
Descriptive Properties Value Comments
Cold Flexibility, °C max -30
Insolubles in toluene, 325 mesh, % max 0.1