Polymer Property : Ring & Ball Softening Point = 266 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point >= 130 °C
>= 266 °F
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer); ASTM D-36
Dynasol Solprene® 411 Thermoplastic Rubber SBS Dry
Solprene 411 is a 70/30 butadiene/styrene thermoplastic copolymer, polymerized in solution and has a radial structure.This product is available in:S 411 porous crumbS 411M powder form dusted with am..
Ring & Ball Softening Point >= 130 °C
>= 266 °F
Modified Bitumen Property in waterproof membranes (150/200 bitumen + 12% polymer); ASTM D-36
Dynasol Calprene® 411 Thermoplastic Rubber SBS Dry
Calprene 411 is a 70/30 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and has a radial structure.This product is available in:C 411 porous crumbC 411C porous pelletC 411M powder..