Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Dynasol
Trade Name Solprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene 9618 is a 69/31 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It is stabilized with non-staining antioxidant system. This product is presented as a free flowing porous pellet for easy handling and dissolution.Uses: Solprene 9618 is designed to be used in high performance adhesive formulations. Main Applications: AdhesivesPolymer modificationInformation provided by Dynasol.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D5668
Brookfield Viscosity 0.60 cP
0.60 cP
25% in toluene; ASTM D2994
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
DIN 53505
Tensile Strength 8.00 MPa
1160 psi
ASTM D412
Elongation at Break 850 %
850 %
ASTM D412
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -66.0 °C
-86.8 °F
ASTM E-1356
Chemical Properties Metric English Comments
Styrene Content 29 %
29 %
Block; NM 202-07
31 %
31 %
NM 300-14