Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.00 - 13.0 MPa | 1160 - 1890 psi | molded; ASTM D4745 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Addisilâ„¢ 1080 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ Electro 242-2 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2660 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3785/30 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4030 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4640 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | >= 8.00 MPa | >= 1160 psi | ASTM F152 |
Thermoseal RG-S160 PTG Gasketing Thermoseal RG-S160 offers exceptional sealability and crush resistance in a wide range of applications. RG-S160 is composed of a blend of aramid, mineral, and cellulose fibers and graphite and other.. |
|||
Tensile Strength | 8.00 MPa @Strain 300 % |
1160 psi @Strain 300 % |
ISO 37 |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 8.00 MPa @Strain 300 % |
1160 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 8.00 MPa @Strain 300 % |
1160 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | fill; ISO 37 Type 2 |
Rogers Corporation Bisco® A2 R 3.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | Flatwise |
Henkel Hysol EA 9257 Primer Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | Flatwise |
Henkel Hysol EA 9657 Film Adhesive High temperature, service film adhesive designed for high honeycomb peel in a reticulated sound suppression structure. Qualified to BMS 5-137. Data from .080 psf, 400 g / m2.Applications: Composite .. |