Material Notes:
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and delivers optimal reinforcement to the plastic matrix in contrast to conventional short glass fiber-reinforced thermoplastics. Molded parts made of SEPAZ LFT are used in virtually every sector of consumer and industrial manufacturing, including automotive, recreation & sports, marine, food & beverage.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength 93.195 MPa
13517 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 122.63 MPa
17786 psi
ASTM D790
Flexural Modulus 5.1012 GPa
739.87 ksi
ASTM D790
Izod Impact, Notched 2.94 J/cm

@Temperature -30.0 °C
5.51 ft-lb/in

@Temperature -22.0 °F
ASTM D256
2.94 J/cm

@Temperature 23.0 °C
5.51 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 210 - 220 °C
410 - 428 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Users viewing this material also viewed the following: