Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | >= 2.94 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 5.51 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5205R PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Izod Impact, Notched | >= 2.94 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 5.51 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY SC1004AU PC, High Impact Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
5.51 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature -40.0 °C |
5.51 ft-lb/in @Temperature -40.0 °F |
3.2 mm (0.125 in) notch |
Kraton® G1702 + PC blend (5/95) Blending KRATON D and G polymers with PC significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | >= 2.94 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 5.51 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
5.51 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
5.51 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature 0.000 °C |
5.51 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PWI High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, reduce heat conductivity to waterRecommended Applications: Above ground pipes, double wall pipesInforma.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.35 mm |
5.51 ft-lb/in @Thickness 0.250 in |
|
TPI Porene® ABS-SR101 High Impact Extrusion Grade ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature 23.0 °C |
5.51 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature -30.0 °C |
5.51 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.40 mm |
5.51 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM11GMS ABS Injection Molding Grade High Rigidity, High Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 6.40 mm |
5.51 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature -30.0 °C |
5.51 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LC30 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.94 J/cm @Temperature 23.0 °C |
5.51 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LC30 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | >= 2.94 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 5.51 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.94 J/cm @Thickness 3.20 mm |
5.51 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |