Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAMID® H12T Unreinforced High Impact PA/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® H12T Unreinforced High Impact PA/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/ABS alloy (Unreinforced, GF reinforced, MR reinforced)Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 0.98 %

@Time 86400 sec
0.98 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength 61.803 MPa
8963.8 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 98.1 MPa
14200 psi
ASTM D790
Flexural Modulus 2.1582 GPa
313.02 ksi
ASTM D790
Izod Impact, Notched 1.37 J/cm
2.57 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F