ELASTO UK Dryflex® 8004-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 8004-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thus will support a wide and flexible range of products.Flame retardant compounds will extend the application areas where resistance to ignition and burning are important features, while their performance characteristics in processing and finished component operation are of the same standard a the Dryflex® general-purpose grades.The flame retardant compounds show an excellent resistance to a variety of polar fluids, such as water, aqueous systems and alcohols. However, in non-polar fluids, such as oil, resistance diminishes with increasing aromatic content. Weathering, including UV stability and ozone resistance is excellent.Conforms to the 750®C glow wire requirements of BS 1363.Processing: The flame retardant grades of Dryflex® can easily be processed using conventional thermoplastic equipment for injection molding as well as other fabricating methods. The thermoplastic characteristics result in faster processing times and complete scrap recycling. The flame retardant compounds do not require pre-drying prior to processing.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ISO 2781
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength at Break 20.0 MPa
2900 psi
ISO 37
Elongation at Break 300 %
300 %
ISO 37
Descriptive Properties Value Comments
Basis Halogen Free
Color Black