EMS-Griltech Grilon® BM 20R Nylon 6 Monofilament (Medium-Set)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® BM 20R Nylon 6 Monofilament (Medium-Set).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON BM 20R is a Nylon 6 based monofilament for press felt fabric and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Filament Diameter 250 - 550 µm
250 - 550 µm
Mechanical Properties Metric English Comments
Elongation at Break 35 - 50 %
35 - 50 %
Tenacity 0.439 - 0.526 N/tex
4.97 - 5.96 g/denier
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Shrinkage 11.0 - 14.0 %

@Temperature 180 °C
11.0 - 14.0 %

@Temperature 356 °F
Thermo Shrinkage
Descriptive Properties Value Comments
Heat Setting Medium-Set