EMS-Griltech Grilon® BN 20R Nylon 6 Monofilament (Non-Set)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® BN 20R Nylon 6 Monofilament (Non-Set).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON BN 20R is a Nylon 6 based monofilament for press felt fabric and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Filament Diameter 200 - 1200 µm
200 - 1200 µm
Mechanical Properties Metric English Comments
Elongation at Break 30 - 45 %
30 - 45 %
Tenacity 0.351 - 0.526 N/tex
3.98 - 5.96 g/denier
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Shrinkage 14.0 - 17.0 %

@Temperature 180 °C
14.0 - 17.0 %

@Temperature 356 °F
Thermo Shrinkage
Descriptive Properties Value Comments
Heat Setting Non-Set