Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ERG Aerospace Duocel® Aluminum Metal Foam

Category Metal , Metal Foam, Mesh, or Honeycomb , Nonferrous Metal , Aluminum Alloy , Other Engineering Material , Composite Core Material
Manufacturer ERG Aerospace
Trade Name Duocel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ERG Aerospace Duocel® Aluminum Metal Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.0810 - 0.324 g/cc
0.00293 - 0.0117 lb/in³
Practical production range 3 - 12% relative density
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.24 MPa
180 psi
For 8% nominal density aluminum foam
Modulus of Elasticity 0.0480 - 0.0830 GPa
6.96 - 12.0 ksi
Compressive Yield Strength 2.17 MPa
315 psi
For 8% nominal density aluminum foam
Compressive Modulus 0.0690 - 0.114 GPa
10.0 - 16.5 ksi
Shear Modulus 0.121 - 0.345 GPa
17.5 - 50.0 ksi
Thermal Properties Metric English Comments
Specific Heat Capacity 0.895 J/g-°C
0.214 BTU/lb-°F
Thermal Conductivity 9.70 W/m-K
67.3 BTU-in/hr-ft²-°F
Melting Point 660 °C
1220 °F
Users viewing this material also viewed the following: