Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 762 Nickel Silver 12%, Extra Spring

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 762 Nickel Silver 12%, Extra Spring.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long shelf life. Typical uses include springs for relays, condensers, and decorative belt buckles.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T >= 81
>= 81
Thickness > 0.020 Inch
Tensile Strength, Ultimate >= 786 MPa
>= 114000 psi
Tensile Strength, Yield >= 703 MPa
>= 102000 psi
0.2% offset
Elongation at Break <= 1.0 %
<= 1.0 %
in 2 in.
Tensile Modulus 124 GPa
18000 ksi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 20.0 - 300 °C
9.00 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 41.5 W/m-K
288 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 59 %
59 %
Nickel, Ni 12 %
12 %
Zinc, Zn 29 %
29 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000198 ohm-cm
0.0000198 ohm-cm
Annealed
Users viewing this material also viewed the following: