Eastman Aqua PJ002 PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Eastman Chemical
Trade Name Aqua
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Aqua PJ002 PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer PJ002 is a clear copolymer with an I.V. of 0.8.Applications/UsesWater bottles
Physical Properties Metric English Comments
Bulk Density 0.817 g/cc
0.0295 lb/in³
ASTM D1895
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <3ppm
VKCA-A-AS-G-GC-0001
Color, CIE a* -2.5 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE b* 0.3 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE L* 77.5 MIN
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05