Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 464 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
Omnia Plastica Akulon® PA 66.6 - Akulon GX - at 50% RH
Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool..
Melting Point 240 °C
464 °F
ISO 11357-3
Pasargad Polymer Peyvand Pasalac 3P-H6000B ABS
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly..
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Eastman PG400 PET  (discontinued **)
Voridian PET PG400 is a general purpose resin is mostly supplied into Mexico and has a wide array of applications in container manufacturing.Applications/UsesBeverage packagingContainersFood packagi..
Melting Point 240 °C
464 °F
Average value: 240 °C Grade Count:10
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Melting Point 240 °C
464 °F
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Melting Point 240 °C
464 °F
MPC Method
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade  (discontinued **)
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Melting Point 240 - 271 °C
464 - 520 °F
Average value: 255 °C Grade Count:6
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum..
Melting Point 240 °C
464 °F
crystalline melting point; ASTM D4591
Honeywell Halar® High Performance E-CTFE Film  (discontinued **)
Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem..
Melting Point 240 °C
464 °F
C-120
I. Stern IS-7985 Polyethylene Terephthalate Resin
Product Description: IS-7985 is a natural polyethylene terephthalate (PET) resin. This resin is produced by continuous melt phase polymerization followed by solid phase polymerization.Certificatio..
Melting Point 240 °C
464 °F
Target; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ Plus 1111 PET Resin
Description: La resina Polyclear® Plus PET 1111 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen un..
Melting Point 240 °C
464 °F
Target; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ Refresh 1101 PET Resin
Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen..
Melting Point 240 - 242 °C
464 - 468 °F
SK Chemicals SKYPET® BB8055 Specially Formulated PET Resin
Description: SKYPET-BB8055 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB8055 provides excellent processability in injection molding and blow mol..
Melting Point 240 °C
464 °F
DSC
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin
Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p..
Melting Point 240 - 264 °C
464 - 507 °F
Williams Advanced Alloys WS264 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Eastman Aqua PJ002 PET
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer PJ..
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Eastman Aqua PJ003 PET
Voridian Aqua PET PJ003 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. This product is specifically designed f..
Melting Point 240 °C
464 °F
DIN 53765
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Conditioned)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Melting Point 240 °C
464 °F
DIN 53765
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry)
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector..
Melting Point 240 °C
464 °F
DIN 53765
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry)
Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire ..
Melting Point 240 °C
464 °F
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)  
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Melting Point 240 °C
464 °F
MPC Method
Mitsui TPX® MX004 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Melting Point 240 °C
464 °F
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Melting Point 240 °C
464 °F
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)  (discontinued **
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Melting Point 240 °C
464 °F
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Copyright © lookpolymers.com All Rights Reserved