Material Notes:
Voridian PET PG400 is a general purpose resin is mostly supplied into Mexico and has a wide array of applications in container manufacturing.Applications/UsesBeverage packagingContainersFood packaging
Physical Properties Metric English Comments
Bulk Density 0.817 g/cc
0.0295 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
Intrinsic; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <3ppm
VKCA-A-AS-G-GC-0001
Color, CIE a* -2.5 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE b* 0.3 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE L* 77.5 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
VGAS-A-AN-G-GA-1
Pellet Shape Cubical