Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene

Category Polymer , Thermoplastic , Polymethylpentene (PMP)
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.90 g/cc
3.90 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.63 MPa
2412 psi
ASTM D638
Elongation at Break <= 1.0 %
<= 1.0 %
ASTM D638
Tensile Modulus 3.17 GPa
460 ksi
ASTM D638
Flexural Strength 14.5 MPa
2100 psi
ASTM D790
Flexural Modulus 2.217 GPa
321.6 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.7 °C
197 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.4 °C
202 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 274 - 302 °C
525 - 575 °F
Mold Temperature 57.2 - 82.2 °C
135 - 180 °F