Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 94.4 °C | 202 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AS-1000 Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:UnfilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.5 °C | 202 °F | Annealed (2 hours at 80°C); ISO 75 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.4 °C | 202 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8009 FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.4 °C | 202 °F | Annealed; ASTM D648 |
Total PSI 940E Impact Polystyrene Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination of high gl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.4 °C | 202 °F | ASTM D648 |
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers |