Material Notes:
High Specific GravityStainless Steel Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 4.00 g/cc
4.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.00 MPa
2756 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Flexural Modulus 8.631 GPa
1252 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 204 - 249 °C
400 - 480 °F
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Dry Time 2 - 4 hour
2 - 4 hour