Eifeler Coatings Technology CROSAL® AlCrN PVD Coating

Category Ceramic , Nitride , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name CROSAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology CROSAL® AlCrN PVD Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This unique AlCrN based high performance coating has specially been developed for applications at high or highest temperatures.Information provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 2.00 - 5.00 microns
0.0787 - 0.197 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 2900 - 3500
2900 - 3500
Coefficient of Friction 0.45
0.45
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1100 °C
2010 °F
Descriptive Properties Value Comments
Color slate-grey