Polymer Property : Thickness = 0.0787 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
General plating (excluding exotic metals)
Parker Chomerics SPRING-LINE® Beryllium-Copper Gasket
Description: SPRING-LINE beryllium-copper gaskets combine high levels of EMI shielding effectiveness with spring-finger wiping and low closure force properties. The high performance qualities of ber..
Thickness 2.00 - 10.0 microns
0.0787 - 0.394 mil
Möller Medical TafSkin 109 L NanoCoating
Electrically conducting, chemical-resistant, thin, easy-to-clean PTFE coatingInformation provided by Möller Medical, Member of CENTROTEC Group
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
Eifeler Coatings Technology CrCN PVD Coating
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal..
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
Eifeler Coatings Technology CrN PVD Coating
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal..
Thickness 2.00 - 5.00 microns
0.0787 - 0.197 mil
Eifeler Coatings Technology CROSAL® AlCrN PVD Coating
This unique AlCrN based high performance coating has specially been developed for applications at high or highest temperatures.Information provided by Eifeler Coatings Technology
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology EXXTRAL® plus PVD Coating
Key Characteristics: high hardness, very good oxidation resistance, low thermal conductivityPrimary Applications: machining of hardened steel and thicker steel sheets; excellent chemical resistance;..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology EXXTRAL® rose PVD Coating
Key Characteristics: high hardness and elasticity, low friction, high oxidation resistancePrimary Applications: excellent for stainless steel and nickel-based high temperature alloys; hard and copy ..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology EXXTRAL® silver PVD Coating
Key Characteristics: high hardness, good oxidation resistance, low frictionPrimary Applications: machining of abrasive or sticking materials (stainless steel, cast iron, Si-rich Al-alloys); machinin..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology SISTRAL® AlTiN PVD Coating
Key Characteristics: extreme wear resistance at high temperature, excellent oxidation resistancePrimary Applications: excellent choice for cutting under extreme conditions (hard abrasive materials, ..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology SUPRAL TiAlN PVD Coating
A TiAlN-based hard coating, especially developed for drilling under extreme conditions.Information provided by Eifeler Coatings Technology
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology TiCN PVD Coating
Key Characteristics: high hardness excellent abrasive wear resistance, enhanced toughnessPrimary Applications: machining of difficult to machine alloy steels; high performance cutting where moderate..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology TiN PVD Coating
Key Characteristics: standard all purpose coatingPrimary Applications: machining / cutting of iron based material; metal forming; plastic molding of highly abrasive plastics; orthopedic instrumentat..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology VARIANTA® TiAlN PVD Coating
Key Characteristics: high hardness, very good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of cast iron and nickel base..
Thickness 2.00 - 4.00 microns
0.0787 - 0.157 mil
Eifeler Coatings Technology VARIANTIC® TiAlCN PVD Coating
Key Characteristics: low friction, good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of all types of steel under dry as..