Eliokem Chemigum® P615D Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eliokem
Trade Name Chemigum®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eliokem Chemigum® P615D Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium viscosity grade for friction materials. 33% bound ACN. Linear polymer structure. CaCO3 partitioning agent.Can be used in phenolic blends.Used in friction materials such as disc-pads, clutch facings, and brake linings. Also used in solvent & wet process fiber gaskets and in solvent-based adhesives.Information provided by Eliokem.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Particle Size 800 µm
800 µm
Median
Mooney Viscosity 50

@Temperature 100 °C
50

@Temperature 212 °F
ML 1+4