Elisto THERMOSTAR® LC 6000 Insulation Material

Category Other Engineering Material
Manufacturer Elisto
Trade Name THERMOSTAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elisto THERMOSTAR® LC 6000 Insulation Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pattern material. Insulation materials for mechanical engineering.Information provided by elisto
Mechanical Properties Metric English Comments
Flexural Strength 150 MPa

@Temperature 23.0 °C
21800 psi

@Temperature 73.4 °F
Compressive Strength 100 MPa

@Temperature 200 °C
14500 psi

@Temperature 392 °F
340 MPa

@Temperature 23.0 °C
49300 psi

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C
392 °F