Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 250 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 482 °F |
|
Pyrotek Wollite 37 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
Thermal Conductivity | 0.140 - 1.76 W/m-K | 0.972 - 12.2 BTU-in/hr-ft²-°F | Average value: 0.570 W/m-K Grade Count:22 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® FL920 PC (Europe-Africa-Middle East) LEXAN FL920 is a foamable grade of LEXAN polycarbonate, containing 20% glass-fibre is designed of applications where superior flexural and tensile charasterics are required. LEXAN FL920 also offers .. |
|||
Thermal Conductivity | 0.140 - 0.190 W/m-K | 0.972 - 1.32 BTU-in/hr-ft²-°F | Average value: 0.162 W/m-K Grade Count:4 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Thermal Conductivity | 0.140 - 1.28 W/m-K | 0.972 - 8.88 BTU-in/hr-ft²-°F | Average value: 0.510 W/m-K Grade Count:28 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene) Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics Corzan® PVC-C Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | ASTM C177 |
CPC - Vycom Corzan® CPVC Chlorinated PVC Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | ASTM C177 |
CPC - Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet Flametec™ CPVC made from Corzan® 4910 white 120 compound is a high heat, corrosion resistant chlorinated polyvinyl chloride sheet. Because of its excellent corrosion resistance at elevated tempera.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti.. |
|||
Thermal Conductivity | 0.140 W/m-K @Temperature 50.0 °C |
0.972 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
3M S42XHS Glass Bubbles 3M™ Glass Bubbles S42XHS are high-strength additives for polymers made from a water-resistant and chemically stable sodalime-borosilicate glass. These hollow glass microspheres can be compounded wi.. |
|||
Thermal Conductivity | 0.140 - 0.170 W/m-K | 0.972 - 1.18 BTU-in/hr-ft²-°F | |
Hippe PVC-U Polyvinyl Chloride Material at reasonable price, high strength. Used in machine construction as covers, pipes, section, façade elements.Information provided by Hippe. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Thermal Conductivity | 0.140 W/m-K | 0.972 BTU-in/hr-ft²-°F | |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Thermal Conductivity | 0.140 - 0.390 W/m-K | 0.972 - 2.71 BTU-in/hr-ft²-°F | Average value: 0.284 W/m-K Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |