Elmer's Products Aron Alpha® 403T Cyanoacrylate Adhesive (Industrial Krazy Glue™)

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Elmer's Products, Inc.
Trade Name Aron Alpha®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elmer's Products Aron Alpha® 403T Cyanoacrylate Adhesive (Industrial Krazy Glue™).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fair on porous substrates. Superior impact resistance. Superior peel resistance. Very good thermal shock resistance. A primer is required for hard-to-bond materials such as polyethylene, polypropylene, acetal, PET, nylon, soft PVC, silicone rubber, and glass.General information about the Aron Alpha® product line: Cyanoacrylates are single component instant adhesives that bond a wide variety of surfaces with a strong, durable bond. They offer ease of application, a wide range of performance parameters, and reliable solvent-free bonding.Toagosei Co., Ltd. produces cyanoacrylates in Japan, marketed as Aron Alpha® in Japan, Cyanolit® in Europe, and Krazy Glue® in the US. Elmer's Products markets Krazy Glue® to the retail trade and Aron Alpha® to the industrial trade in North America. Information provided by Elmer's Products, Inc.
Physical Properties Metric English Comments
Viscosity 1000 cP
1000 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 30 s set time
29.6 MPa
4300 psi
vs. rigid PVC; 30 s set time
32.4 MPa
4700 psi
vs. steel; 90 s set time
34.5 MPa
5000 psi
vs. polycarbonate; 15 s set time
36.5 MPa
5300 psi
vs. aluminum; 120 s set time
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Estimated; Manufacturer specifies clear but does not quantify.
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
typically used at ambient temperature
Descriptive Properties Value Comments
Color Clear