Engineered Syntactic Systems MZ-38 Deep Water Syntactic Foam

Category Polymer
Manufacturer Engineered Syntactic Systems
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Syntactic Systems MZ-38 Deep Water Syntactic Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high compressive and hydrostatic strengths. This yields a product able to withstand the high hydrostatic pressures experienced by today’s manned and unmanned subsea vehicles.The MZ Grade of syntactic safely operates in the oceans Mesopalegic Zone, down to depths of 1,000 meters. (3280 feet). This group of syntactics is produced using the same technology as the Navy’s submarine void filling materials. This workhorse foam system has been thoroughly tested both during development and during its long history in service. It has been found to be a safe, reliable, cost effective buoyancy source for the relatively shallow requirements for a syntactic. Each block is cast as a single unit, but may be cut to fit the application requirement. Blocks or trimmed parts may also be bonded together to form a larger structure.
Physical Properties Metric English Comments
Density 0.577 - 0.641 g/cc
0.0208 - 0.0231 lb/in³
Water Absorption <= 3.0 %

@Time 86400 sec
<= 3.0 %

@Time 24.0 hour
at depth
Mechanical Properties Metric English Comments
Compressive Strength 29.8 MPa
4320 psi
Compressive Modulus 1.34 GPa
195 ksi
Hydrostatic Design Basis 41.4 MPa
6000 psi
Hydrostatic Crush Strength
Descriptive Properties Value Comments
Service Depth (feet) 3295
Service Pressure (psi) 1450