Polymer Property : Compressive Strength = 4320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 29.8 MPa
4320 psi
Engineered Syntactic Systems MZ-38 Deep Water Syntactic Foam
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having..