Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, PTFE-Filled
Manufacturer Ensinger
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a variety of applications prmarily on submarines. This advanced acetal material uses a combination of PTFE fibers uniformly dispersed in Delrin acetal resin. The combination results in improved wear characteristics along with strength, toughness, dimensional stability and machinability. The profile also yields a material with superior load bearing capabilities, especially when operating at high speeds.Developed specifically for US Naval useMeets requirements for NAVSEA 5959311 rev C and NAVSEA 803-4384678 rev B and CMeets requirements per General dynamics Dwg. 4384678 rev C note 7 with Drn C2All stock shapes are traceable to resin lot and batchDELRIN® DE588 is designed and approved specifically for naval applications and is suitable in a variety of uses such as bushings, bearings, seals, gaskets and valve seats.Information provided by Ensinger
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D638
2.50 GPa
363 ksi
injection molded samples; ASTM D638
Compressive Strength 14.5 MPa

@Strain 1.00 %
2100 psi

@Strain 1.00 %
ASTM D695
75.8 MPa

@Strain 10.0 %
11000 psi

@Strain 10.0 %
ASTM D695
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Tensile Impact Strength 10.5 kJ/m²
5.00 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ASTM D3418
Maximum Service Temperature, Air 85.0 °C
185 °F
long term
149 °C
300 °F
intermittent
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
244 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: