Material Notes:
Heat Stabilized nylon, increased ability to withstand the negative effects of heat exposure and increased overall service temperature over nylon 6/6.Information provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
Users viewing this material also viewed the following: