Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Ensinger
Trade Name Tecapeek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ASTM D792
Filler Content 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Tensile Strength 97.2 MPa
14100 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
3.0 %
3.0 %
Flexural Strain; ASTM D790
Tensile Modulus 5.86 GPa
850 ksi
ASTM D638
Flexural Strength 149 MPa
21600 psi
ASTM D790
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 374 °C
705 °F
DSC
Descriptive Properties Value Comments
Color Black