Mechanical Properties Metric English Comments
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
PolyOne Maxxam™ PPR-30G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
PolyOne Maxxam™ PPR-30G Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
PolyOne Maxxam™ X MX5210-0030 RS Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Techmer ES Elastoblend® PA6 GF15 IM HS L 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Techmer ES Elastoblend® PA6 GF18 IM 511 18% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Flexural Modulus 5.03 GPa
730 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM AR9100 PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Flexural Modulus 5.03 GPa
730 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® DR48 PBT
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
Flexural Modulus 5.03 GPa
730 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific)
17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA.
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc.
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Techmer ES HiFill® PA6 GF/M30 HS BK 10/20% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat ..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Information provided by Star Plastics, Inc.
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6
LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0600R 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 5.03 GPa
730 ksi
ISO Data
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Flexural Modulus 5.03 GPa
730 ksi
ISO Data
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t..
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0600 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-1804 30% Glass Fiber Reinforced, Heat and UV
Information provided by Asahi Thermofil
Flexural Modulus 5.03 GPa
730 ksi
ASTM D790
Chase Plastics CP Pryme® N233GL (COND, 50% RH) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 5.03 GPa
730 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications.
Flexural Modulus 5.03 GPa
730 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM AR9100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.