Material Notes:
This product is intended for use in injection molding applications for automotive and consumer products and also contains a long-term heat aging additive package.Information provided by Entec
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus, 1% Secant 1070 MPa
155000 psi
ASTM D790
Izod Impact, Notched >= 3.20 J/cm

@Thickness 3.17 mm
>= 5.99 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648