Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ FR MF5420-0085 NHFR Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ PP-16CP/000-2 HI Polypropylene, Unspecified (PP, Unspecified) Stat-Tech™ electrically conductive compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic applications. These compounds combine .. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® X11 ABS Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Asia Pacific) Weatherable, injection moldable ASA+PC blend. In a wide range of colors. Recommended for unpainted exterior/high heat applications. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
5.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm |
5.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Apec® DP9-9343 High-Heat Polycarbonate, UV Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 3.20 - 7.50 J/cm | 5.99 - 14.1 ft-lb/in | Average value: 4.64 J/cm Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Rostone Rosite® 3552C BMC Thermoset Polyester, 15% Glass Reinforced
(discontinued **) Key Features: High Stability, Non-OutgassingDesigned for applications requiring excellent stability and dimensional control. Out-gassing is virtually eliminated making it ideal for systems such as .. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Ineos K44-08-123 HDPE Copolymer with Carbon Black Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Ineos K44-15-122 HDPE K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Ineos K44-08-122 HDPE K44-08-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as havin.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GP 100 OR HDPE The resin GP 100 OR is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256-93a |
Multibase Multi-ABS 3365 High Impact ABS Data provided by Multibase. |
|||
Izod Impact, Notched | 3.20 J/cm @Temperature 23.0 °C |
5.99 ft-lb/in @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Astryn EPKT25M Polypropylene Copolymer, Mineral Filled Key Features: conventional melt flow, very high modulus, mineral-filled polypropylene copolymer, high rigidity, good impact resistance, good dimensional stability, low foggingApplications: glove box.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1543 PPE+PS (Asia Pacific) |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EM6101 PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 250F DTUL. Good property retention/wide temperature range. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Izod Impact, Notched | >= 3.20 J/cm @Thickness 3.17 mm |
>= 5.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-CP8/6 Impact Copolymer, 8 Melt Flow This product is intended for use in injection molding applications for automotive and consumer products and also contains a long-term heat aging additive package.Information provided by Entec |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM-D256 |
Braskem GM8250 HDPE Blow Molding Polyethylene GM8250 is a high-density polyethylene that has high molecular weight, excellent tenacity, high stiffness, good impact resistance, and good environmental stress cracking resistance. It was developed .. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | |