Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Porocell POR 301/F NR-SBR Foam

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Eurofoam s.r.l.
Trade Name POROCELL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Porocell POR 301/F NR-SBR Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 40 - 50
40 - 50
ASTM D 2240
Tensile Strength 0.500 MPa
72.5 psi
ASTM D 412
Elongation at Break >= 100 %
>= 100 %
ASTM D 412
Compressive Yield Strength 0.0500 MPa

@Strain 25.0 %
7.25 psi

@Strain 25.0 %
ASTM 1056/85
Tear Strength 0.400 kN/m
2.28 pli
ASTM D 624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
ASTM D 3575
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Vulcanization Peroxide
Users viewing this material also viewed the following: