Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0500 MPa | 7.25 psi | at 30% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ M DM-710A Foam Polyurethane MDI backbone: ether.Shore 00 Hardness: 55Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Compressive Yield Strength | 0.0500 MPa | 7.25 psi | at 10% Compression, Parallel to thickness |
Zircar Ceramics AXL Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |
|||
Compressive Yield Strength | 0.0500 MPa @Strain 25.0 % |
7.25 psi @Strain 25.0 % |
ISO 7214 |
Zotefoams ZOTEK® F 30 PVDF Foam Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Compressive Yield Strength | 0.0500 MPa @Strain 25.0 % |
7.25 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Polycell PLZ 45 Polyethylene Foam Information provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.0500 MPa @Strain 25.0 % |
7.25 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 301/F NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |