Material Notes:
Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and surface printed) horizontal or vertical packaging applications. It is also used as an outer web of laminations for vertical gas-flush applications.Availability: Latin America, North America and South AmericaKey Features:Robust machinabilityLow and consistent COFOutstanding optical propertiesExcellent barrier performanceOutstanding flavor and aroma barrierExcellent moisture barrierExcellent oxygen barrierFeatures:Acrylic CoatedFlavor & Aroma BarrierGas BarrierHigh Barrier Printable PVdC CoatedHigh Barrier PVdC CoatedIn Lamination Lap SealableMoisture BarrierOxygen BarrierPVdC CoatedSealable High Barrier PVdC CoatedApplications:BakeryBiscuits/Cookie/CrackersBox OverwrapConfectionery, GumConfectionery, SugarPet FoodUses:Box Overwrap Flexible PackagingHFFS Flexible PackagingPre-made Bags - Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 2.50 g/m²/day
0.161 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Oxygen Transmission Rate 6.20 cc/m²/day
0.399 cc/100 in²/day
23°C, 0% RH; ExxonMobil Method
Thickness 27.9 microns
1.10 mil
Nominal; ExxonMobil Method
Coating Weight 25.1 g/m²
15.7 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.28
0.28
ExxonMobil Method
Film Tensile Strength at Break, MD 117 MPa
17000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 228 MPa
33000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.5 %
4.5 %
at 275°F; ExxonMobil Method
Shrinkage, TD 4.0 %
4.0 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
ExxonMobil Method
Gloss 103 %
103 %
45º; ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 218°F
PVdC/PVdC, 200g/in
Crimp Seal Strength 620 g/in
PVdC/PVdC, 260°F, 20psi, 3/4sec
Yield 27400 in2/lb