Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 27.9 - 43.2 microns | 1.10 - 1.70 mil | Supported Adhesive |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Thickness | 28.0 microns | 1.10 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Thickness | 28.0 microns | 1.10 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm) PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used.. |
|||
Thickness | 27.9 microns | 1.10 mil | |
Hexcel® HexForce™ 104 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Bicor™ 29MB080 OPP Film Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS.. |
|||
Thickness | 27.9 microns | 1.10 mil | |
ExxonMobil Hicor® 110 BIHD-ASB OHD Film One-side acrylic, one-side PVdC coated, oriented high density polyethylene film. This film provides tack seal capability and excellent deadfold. Information provided by ExxonMobil Chemical |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 28LLG MET OPP Film Product Description: A clear, one-side metallized, one-side treated oriented polypropylene film. The metalized layer is designed to provide a bright metal appearance in surface print or laminated ap.. |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 28LLG-202 OPP Film Product Description: A white, two-side treated, polypropylene film designed for use in roll-fed labeling of cylindrical glass, plastic, and metal containers. Typical applications include food, bever.. |
|||
Thickness | 27.9 microns | 1.10 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 29LL210 Preliminary Data Sheet OPP Film Product Description: A biaxially oriented, transparent polypropylene film for pressure sensitive labeling and tape applications.Availability: Africa & Middle East and EuropeKey Features: High yieldG.. |
|||
Thickness | 27.9 microns | 1.10 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 110 ASB-X OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. ASB-X is good for heavy .. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7026 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7042 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7048 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7051 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7214SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M FP032305 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7028FL Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7031 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7033 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7035 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 27.9 microns | 1.10 mil | Facestock |
3M 7037 Screen Printable Polyester Performance Label Product 3M™ Screen Printable Polyester Performance Abel Product 7037 is a durable, high performance material that offers excellent thermal stability and moisture resistance. This polyester label stock util.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7053 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7215SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7218SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7220SA Screen Printable Polyester Performance Label Products with Structured Adhesive 3M™ Screen Printable Polyester Performance Label Products with Structured Adhesive are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topc.. |
|||
Thickness | 27.9 microns | 1.10 mil | Adhesive |
3M 7620/7890 White Vinyl Label Material 3M™ White Vinyl Label Material 7620 / 7890 is a rigid, gloss vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick ta.. |
|||
Thickness | 27.9 microns | 1.10 mil | Backing; ASTM D3752 |
3M 853 Polyester Tape 3M™ Polyester Tape 853 is comprised of strong, thin polyester backing with high shear, solvent resistant acrylic adhesive. These qualities make this tape ideal for applications where solvent exposu.. |
|||
Thickness | 27.9 microns | 1.10 mil | Backing; ASTM D3652 |
3M Scotch® 311 Box Sealing Tape Scotch® Box Sealing Tape 311 is a general purpose box sealing tape designed specifically for utility type applications on light to medium weight boxes. The product offers good performance over broa.. |